Superalloys are indispensable materials in aviation navigation, military industry and so on. The master superalloys smelted by Vacuum induction furnace is one of our main products and its quality has reached advanced level at home and abroad, which can be used for making turbine vanes, guide vanes and other heat resistant components in aviation and other industries. Wrought Superalloys Wire,strip,and bar can also be produesed.

 Mechanical Properties
Condition Tensile Property Stress Rupure Property
Cast Temperature
ºC
Rm
N/mm2
Rp0.2
N/mm2
A
%
Temperature
ºC
Stress
N/mm2
A
%
Life
hr
760±3 >860 >690 >4 871±2 414 >4 >24
Room
Temperature
>780 >680 >2 ---
 